ASTM A336 covers ferritic steel forgings for boilers, pressure vessels, high temperature parts and related equipment.
Forgings made of the steel grades listed in specification A335 / A335m can also be ordered in accordance with this specification.
The chemical, tensile, heat treatment and marking requirements of specification A335 / A335m shall apply.
ASTM Standard for seamless steel pipe:
Executive Standard |
Grade / Material |
Product Name |
A, B |
Black and Hot-Dipped Zinc-Coated Steel Pipes Welded and Seamless |
|
A, B |
Seamless Carbon Steel for High Temperature Service |
|
Low Carbon Steel |
Seamless Cold-Drawn Low-Carbon Steel Heat Exchanger and Condenser Tubes |
|
Low Carbon Steel |
Seamless Carbon Steel Boiler Tubes for High Pressure |
|
ASTM A210 |
A1, C |
Seamless Medium-Carbon and Alloy Steel Boiler and Superheater Tubes |
T5, T11, T12, T22 |
Seamless Ferritic and Austenitic Alloy Steel Boiler, Superheater and Heat-Exchanger Tubes |
|
TP 347H |
||
ASTM A312 |
TP304/304L, TP316/316L |
Seamless Steel Pipe for Stainless Materials |
Gr.6 |
Seamless and Welded Steel Pipe for Low-Temperature Service |
|
P9, P11, P22 |
Seamless Ferritic Alloy Steel Pipe for High-Temperature Service |
|
ASTM A519 |
41,304,140 |
Seamless Carbon and Alloy Steel for Mechanical Tubing |
ASTM A789 |
|
Seamless Ferritic/Austenitic Stainless Steel Tubing for General Service |
API Standard for seamless steel pipe:
Executive Standard |
Grade / Material |
Product Name |
J55, K55, N80, L80,C90, C95, T95, P110, M65 |
Spectification for Casing and Tubing |
|
API Spec 5L PSL1 / PSL2 |
Specification for Line Pipe |
DIN / EN Standard for seamless steel pipe
Executive Standard |
Grade / Material |
Product Name |
DN 17175/EN10216-2 |
ST35, ST45, ST52, 13CrMo44 |
Seamless Steel Tube for Elevated Temperature |
DIN 2391/EN10305-1 |
St35, St45, St52 |
Cold Drawn Seamless Precision Pipe |
DIN 1629/EN10216-1 |
St37, St45, St52 |
Seamless Circular unalloyed Steel Tubes Subject to Special Requirments |
ASTM A336 Heat Treatment :-
1. Except as permitted in ‘point 3’ for Grade F22V, and in ‘point 4’ for Grade F91 and Grade F92, the steel
forgings shall be annealed or normalized and tempered but alternatively may be liquid quenched and
tempered when mutually agreed upon between the manufacturer and the purchaser.
2. For all grades, normalizing or liquid quenching shall be followed by tempering at a subcritical temperature
as shown in table 1.
3. Grade F22V forgings shall be normalized and tempered or liquid quenched and tempered at the
manufacturer’s option. For Grade F22V forgings the minimum austenitizing temperature shall be 1650°F
[900°C].
4. Grade F91 forgings having any section thickness greater than 3 in. [75 mm] shall be normalized and
tempered or liquid quenched and tempered at the manufacturer’s option. Grade F92 forgings shall be
normalized and tempered or liquid quenched and tempered at the manufacturer’s option.
5. For Grade F91, F911, and F92 forgings, the austenitizing temperature shall be in the range of 1900 to 1975°F
[1040 to 1080°C].
6. For Grade F6NM the austenitizing temperature shall be 1850°F [1010°C] minimum.
Conatct us